Abstract
Statement of problemWhether laser-welded (LW) titanium can resist the stress corrosion produced by the combination of fluoride ions and stress in the oral environment is unknown. PurposeThe purpose of this in vitro study was to investigate the influence of stress corrosion on the mechanical properties of LW titanium. Material and methodsTwenty-seven titanium bars (25×2 mm) with a circular cross-section were cut in half and laser-welded, while another 27 nonwelded (NW) bars were used as the control. Thirty bars were submitted to a flexural load of 480 N at 1 Hz and immersed in artificial saliva at pH 6 (S1) or in 1000 ppm fluoride-containing saliva at pH 6.0 (S2) or 2.0 (S3) at room temperature for up to 4000 cycles. After the stress corrosion simulation, the tensile strength and Vickers microhardness were determined (n=5). Twelve LW and NW bars were submitted to the corrosion immersion test media for 51 days (n=2) to determine polarization curves (n=2) in an artificial saliva media. The corroded surface was examined with scanning electron microscopy (SEM). ResultsThe combination of fluoride and low pH significantly decreased the tensile strength of LW (P<.05). Stress corrosion did not affect the hardness of LW or NW (P>.05). NW bars immersed in S3 exhibited progressive surface dissolution, while LW bars spontaneously fractured at the welded area after 25 days of immersion in the same medium. SEM images demonstrated pitting corrosion without the presence of cracks in both groups immersed in S3. ConclusionsStress corrosion caused by acidic fluoride-containing saliva and flexural load cycling decreased the tensile strength and hardness of LW titanium bars.
Talk to us
Join us for a 30 min session where you can share your feedback and ask us any queries you have
Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.