Abstract

AbstractTensile tests were performed on specimens in the normalised and tempered condition to assess the effects of temperature (300 – 873 K) and strain rate (6.33×10−5 − 6.33×10−3 s−1) on tensile deformation and fracture behaviour of 9Cr – 1Mo ferritic steel. At all strain rates, the yield and ultimate tensile strength values exhibited a gradual decrease up to intermediate temperatures followed by a rapid decrease at high temperatures. Elongation to fracture and reduction in area displayed a gradual decrease to a minimum at intermediate temperatures followed by a rapid increase at high temperatures. At intermediate temperatures, 9Cr –1Mo steel exhibited serrated flow, plateaus and peaks in strength values and work hardening rate, and negative strain rate sensitivity. The activation energy estimated from the strain to onset of serrations indicated diffusion of interstitial solutes such as carbon responsible for serrated flow in 9Cr – 1Mo steel. At high temperatures, a systematic decrease in yield and tens...

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.