Abstract

ObjectivesThe aim of this study was to evaluate the influence of storage time on the bond strength of self-etching adhesive systems to artificially demineralized dentin submitted to application of a papain-based chemical mechanical agent for carious tissue removal. Materials and MethodsTwenty-four blocks of human coronal dentin were randomly divided into 2 groups: (1) restored with a two-step self-etching adhesive system (Clearfil SE Bond); (2) restored with a one-step self-etching adhesive system (One-Up Bond F Plus). After artificial caries induction, the specimens were treated with papain-based gel, received an application of the adhesive system according to the respective group, and blocks of microhybrid resin composite measuring 5.0mm high and 5.0mm wide were fabricated incrementally on the tooth, which would later be cut to obtain sticks with a bond area of around 1mm2, for use in the microtensile tests. After this, half of the sticks obtained from each tooth were submitted to the microtensile test 24h later, while the other half were stored in water, in an oven at 37°C for a period of 180d. The specimens were submitted to the microtensile test in a Universal Test Machine at a speed of 0.5mm/min. The surfaces of the fractured test specimens were examined visually under a stereoscopic loupe in order to classify the fracture type. After exploratory analysis of the data, the two-way Analysis of Variance (ANOVA) and the Tukey test were applied. The data on the fracture types were analyzed by the Exact Fisher test. ResultsNo statistically relevant differences were verified among the means of the microtensile bond strength values of the adhesive systems evaluated in the different storage times. Mixed and adhesive fractures types were observed for both groups. ConclusionStorage time did not influence the bond strength of the two-step or one-step self-etching adhesive systems to artificially demineralized dentin submitted to application of a papain-based chemical mechanical agent for carious tissue removal. Both adhesive systems provided similar bond strength at different storage times.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call