Particle size of additive geomaterials could affect the cement–clay reaction, thereby reducing strength. The effects of five particle sizes (A, B, C, D and E: >75, 40–75, 20–40, <20 and < 1–106 µm, respectively) of waste granite powder in cement-treated clay mixed composites were investigated. The effects on the liquid limit, unconfined compressive strength (UCS) and microstructural characteristics were investigated. The particle size influenced the UCS in the order of D > A > C > B, and D exhibited higher UCS than the control sample. The increase in the UCS was due to the increased surface area and pozzolanic reactivity of stone powder D. A reduction in the UCS of cement-treated clay–stone powder E composites occurred as compared to the control sample with a 30% stone powder addition, and equal or improved strength was observed with 50% and 70% additions. Owing to the UCS increment derived from stone powder, we could reduce 28.6% of the cement.
Talk to us
Join us for a 30 min session where you can share your feedback and ask us any queries you have
Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.