Abstract

In order to apply a reduced activation ferritic (JLF-1) steel to the blanket/first-wall structure of a fusion reactor, its fracture toughness is very important for the strict estimation of material life. Fracture toughness testing of irradiated materials requires the use of miniaturised specimens and evaluation of TIG welding (tungsten inert gas arc welding) weldment properties is an important issue because necessary for production of nuclear fusion reactors. In this study, the fracture toughness tests were carried out according to the ASTM E1820-99. It was performed on various sizes (ligament and thickness) and various side-grooves of specimens and the TIG welding joint of JLF-1. The test results showed the standard specimen with side-groove of 40% represented valid fracture toughness. Fracture resistance curve (R-curve) increased with increasing specimen ligament and decreased with increasing specimen thickness. However, the R-curve of half size specimen was similar to that of the standard (1inch thickness) specimen. The fracture toughness test results of the TIG welded specimen showed a slight increase in the TIG welded specimen compared with JLF-1 base metal specimen.

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.