Abstract
The microstructure and mechanical properties of wrought Al-12.7Si-0.7Mg alloy were investigated aiming at understanding the influence of the solution treatmen. The result show that the Si particles were gradually rounded and the grain size increase with increasing the solution temperature from 500°C to 540°C. The alloy in T4 condition changed due to the grain szie, Si particles and the super saturation level of Mg ans Si solute atoms. With higher solution temperature, the volume fraction of the pricipitate becomes more which result in good manchannical properties.
Talk to us
Join us for a 30 min session where you can share your feedback and ask us any queries you have
More From: IOP Conference Series: Materials Science and Engineering
Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.