Abstract

The effect of small amounts of Si and Cr on the high temperature oxidation of alloys based on Co-9Al-9W was investigated at 900 °C. The results show that the effect of Si additions on oxidation resistance was more pronounced than for Cr additions. An addition of 4 at.% Cr was insufficient to produce a protective layer, while 2 at.% Si led to the formation of a dense, continuous Al2O3 scale. The thermodynamics and kinetics for Al2O3 layer formation were analyzed by combining CALPHAD and Wagnerʼs theory.

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.