Abstract

NiO and SDC Powders were Prepared by Sol-Gel Method and then Calcined at 400、600 and 800°C. Nio-SDC Anode Materials were Synthesized by Solid State Reaction According to the Mass Ratio of Nio:SDC=65:35 Ratio . XRD Measurement Showed that Powders Consist of Two Phases, the Cubic Nio and Fluorite Structure Ceria . the Grain Size was Shown to Increase with Increasing Temperature. the Cermet with Ni-SDC Powders Calcined at 400°C Showed the Highest Electric Conductivity and a Lower Degree of Polarization.The Electrical Conductivity was 4155Scm-1and Overpotential was 0.12V at 600°C.

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.