Abstract

Correlation of phase purities, microstructure,Jc and Hc2 with sintering temperature has been studied in Zn-stearate-dopedMgB2/Fe tapes. All doped tapes show significant enhancements inJc and Hc2. TEM analyses revealed that strong flux pinning centers induced by grain boundaries andcrystal defects as well as carbon substitution effect are responsible for the improvement ofJc and Hc2 values. Although a high sintering temperature of850 °C increases the grain size, improved grain connection can compensate for this disadvantage, giving thebest Jc of 2.0 × 104 A cm−2 at 4.2 K and 10 T. On the other hand, tapes sintered at900 °C have alower Jc due to the larger grain size and more MgO impurities.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.