Abstract

To determine the influence of two all-in-one self-etching adhesive systems on shear bond strength of a fissure sealant applied under different enamel surface conditions. A total of 180 bovine enamel specimens were randomly distributed to nine experimental groups, defined by the combination of the sealant application technique (using phosphoric acid, or a self-etching water-based adhesive or a self-etching ethanol and water-based adhesive) and enamel surface conditions (dry enamel, saliva or water contaminated enamel). The specimens were submitted to thermocycling prior to the shear bond strength test. High shear bond strength mean values were obtained with the classic technique for dry enamel (31.47MPa), statistically similar values were obtained when the sealant was combined with a self-etching water-based adhesive, in dry enamel (32.36MPa), and when the sealant was combined with a self-etching water-based adhesive in water contaminated enamel (32.62MPa). Under enamel salivary contamination, the best results were achieved using a water-based adhesive (24.78MPa). In saliva contaminated enamel, the combination of a sealant with a water-based self-etching adhesive can maintain high and satisfactory values of bond strength.

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.