Abstract

An experimental investigation was conducted on the durability of recycled aggregate concretes with the water to binder ratios of 0.26 and 0.60, including chloride ion penetration resistance test, freezing-thawing resistance test and water penetration resistance. Natural aggregate, recycled aggregate untreated and recycled aggregate treated by sulfuric acid solution, were employed. Results indicated that, 3 mol/L acid concentration and the 7 days soaking duration was the optimum to remove the attached mortars in recycled aggregate, and its removal rate could reach to 90.8%. Water penetration resistance, chloride ion penetration resistance and freezing-thawing resistance of concrete with 0.26 W/B was superior to that of concrete with 0.60 W/B. The more pores in the internal of concrete with 0.60 W/B could be attributed to that. Durability of recycled aggregate concrete, incorporating recycled aggregate treated by sulfuric acid solution, was improved. In particular, the improvement in recycled high strength concrete was significant.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.