Mill scale is treated as a waste product by the steel industry, so it is essential to recycle and reuse this waste for recovery of metallic iron and its single oxide derivative. Most of the study in the field of mill scale reduction focuses on the static mill scale reduction. Optimizing the process in dynamic conditions becomes more difficult because of the complexity involved inside the process. In the present method, mill scale having particle size ranges from 106 to 53 µm was converted to single-phase oxide Fe2O3 by blowing pure oxygen at 1100 °C and then it was subjected to a reducing atmosphere of 50% H2 and 50% N2 (1:1) at 875 ± 5 °C at a varying reactor angle from 2° to 5° and different mass flow rates varying from 0.037 to 0.148 kg/min. A generalized experimental model (GEM) has been formulated for the degree of reduction of oxide, which encompasses twelve parameters consisting of reactor design and process parameters. A Buckingham theorem was used to obtain dimensionless parameter for the degree of reduction, and a logical correlation using the proposed model has been established.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.