Abstract
Matched samples were obtained from green birch (Betula pubescens) wood. Prefreezing was done at -20°C for 72hours. Both the prefrozen and unfrozen samples were dried and soaked in water for the determination of sorption behavior, swelling properties and fibre saturation point. Prefreezing resulted in 6.7 to 666.7% increase in rate of adsorption, 0 to 13.3% decrease in the rate of desorption, 2.2% decrease in volumetric swelling coefficient and 0.8% decrease in fibre saturation point. However only the change in the rate of water adsorption is statistically significant at 95% confidence level.Since these results were obtained from samples taken from a typical board, more results are required in order to characterise the effects of prefreezing on available stock of Birch wood.
Talk to us
Join us for a 30 min session where you can share your feedback and ask us any queries you have
Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.