Abstract
In this investigation, AA2024 alloy was welded by tungsten inert gas welding. Access the influence of pitting corrosion on TIG weld; the joints were heat-treated after welding with different techniques. Moreover, the corrosion test was carried out with 3.5% NaCl solution under different pH values such as pH:5, pH:7, and pH: 12. From the experimental results, the joint treated with solution treatment with pH: 7 showed high corrosion resistance than its counterparts.
Talk to us
Join us for a 30 min session where you can share your feedback and ask us any queries you have
Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.