Abstract

Annual growth ring width was considered relative to the mechanical properties of timber from the Silesian Forestry Region in Poland. The timber was acquired from raw wood aged approximately 120 years old, with log quality A, B, and C. The study was conducted on 210 pieces of timber; 70 of them were from each part of the log: butt, middle, and top. The tested parameters, modulus of elasticity (MOE) and modulus of rupture (MOR), were measured on fully dimensional timber (40 × 138 × 3500 mm3) that had been dried and planed in industrial conditions. The density of wood (stereometric method) and annual rings width were calculated after MOR and MOE determination on samples including the entire cross-section cut near the failure zone. The tests revealed that the correlation between the width of growth rings and MOE or MOR depended on the log area: it was the highest for timber from butt logs and the lowest for timber from top logs. Moreover, the correlation between growth ring width and MOE or MOR depended also on the quality class of the logs from which the samples were obtained: it was the highest for timber from class A, and the lowest for class C.

Full Text
Published version (Free)

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call