Abstract

Given the shortage of coal with good coking properties, a petroleum coking additive is introduced in coal batch so as to expand the range of plasticity. This additive improves coke quality in every respect, except the total sulfur content. Measures to reduce the additive’s negative impact on the coal pitch are considered.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.