Abstract
In this work, we investigated the influence of passivation coating of aluminum oxide on cycle life of lithium-ion batteries. Al2O3 was synthesized by atomic layer deposition directly on the porous electrodes based on LiCoO2. More than 800 charge-discharge cycles were done. No increase of internal resistance due to Al2O3 coating was observed. According to the results, electrodes coated by aluminum oxide have better cycle life.