Abstract
Abstract High quality Al-doped ZnO (AZO) films are advantageous for many applications. Their properties can be tuned by controlling the doping concentration and intrinsic defect density. In this work, high-quality AZO films have been synthesized using the atomic layer deposition (ALD) technique. Throughout the doping cycle and post-annealing treatments under various atmospheres, the oxygen-related vacancies were controlled. The effect of oxygen vacancies on the charge transportation and surface potential were studied. The O 1s X-ray photoelectron spectrometry (XPS) spectra of the AZO film were deconvoluted into three components related to the O 2 − species, corresponding to the oxygen in the ZnO lattice ( O L ); oxygen vacancies or defects ( O V ); and chemisorbed or dissociated ( O C ) oxygen species. In the case of the as-deposited films and films annealed under various atmospheres, a co-relationship between the O V and mobility ( μ ) can be determined. In the case of the N 2 -annealed film, the O V fraction is at its maximum value, while the other components are at their minimum values. Among the as-deposited films, the maximum O V fraction is obtained when a Al:Zn ratio ( R Al/Zn ) of 7% is used. When R Al/Zn = 7%, the μ value of the as-deposited AZO film is enhanced from 12.1 cm 2 V −1 s −1 ( R Al/Zn = 3%), to 18.5 cm 2 V −1 s −1 . It shows its potential application as photoanode. The Hall Effect and the XPS analysis of the film reviled a co-relationship between O V and μ with the Al-doping concentration or post annealing atmosphere. Kelvin probe atomic force microscopy (KPFM) was used to evaluate the surface charge potentials of the films. The N 2 -annealed AZO film with R Al/Zn = 3% ( AZO-3-N 2 ) exhibited the maximum negative potential (−115.79 mV); however, the film with R Al/Zn = 7% ( AZO-7-N 2 ) exhibited the maximum positive potential (797.23 mV). Hence, the properties of these films may directly pertain to the bit readout signal and reliability of charge storage and memory applications.
Talk to us
Join us for a 30 min session where you can share your feedback and ask us any queries you have
Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.