Abstract

The influence of oxygen on the characteristics of polycrystalline silicon sheets for solar cells, produced by the spin cast method, has been investigated. It was confirmed that if the oxygen concentration was more than 7.5 X 10 17 atoms/cm 3 after the cell fabrication process, the resistivity of the crystal became higher than before cell fabrication process. To obtain solar cells which have an energy conversion efficiency of more than 10%, the oxygen content should be less than 7.5 X 10 17 atoms/cm 3

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.