We systematically studied the influence of optically active defects on thermal conductivity for polycrystalline diamonds (PCDs) with different colour, crystalline quality and impurity concentrations. The thermal conductivities of PCDs on the growth (top) and nucleation (bottom) surfaces were characterized with 3 ω technique. It is found that the bottom surface shows lower thermal conductivity as compared to the top surface. This could be due to the higher defect density in the bottom surface. Defects analyzed includes non-diamond carbon phase, C–H stretching vibration, Si vacancy, and substitutional nitrogen (Ns 0 ). Our results suggest that, for the top surface, the heat transport is mainly controlled by the concentration of Ns 0 . For the bottom surface, non-diamond carbon phase, Si vacancy, C–H stretch and Ns 0 defects all lead to an obvious reduction in the thermal conductivity. Most importantly, we derived a well fitted equation that estimates the thermal conductivity by optical transmittance, and the equation was demonstrated to be valid at any wavelength in visible region.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.