Seven full scale hydrostatic burst tests were carried out on pipes extracted from an API 5LX52 gas pipeline that contained rectangular and elliptical fillet welded patches and other repairs of different geometries. All breaks took place after widespread yielding. This analysis shows that the patches that generate greater risks are those that: (1) were attached to the pipeline at very low pressure, (2) were placed to repair large defects, (3) are rectangular, long in the direction of the pipe, and narrow, (4) the quality of the weld is doubtful. Based on data reported by In Line Inspection (ILI), of the four conditions mentioned above, only the third can be assessed in order to quantify risks and to schedule replacements.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.