Abstract
Three-pass friction stir processing (FSP) with different moving distances of the stirring tool between the two successive passes, 50% diameter of the pin (traditional way) and 50% diameter of the shoulder (novel way), was conducted on 7B04-O Al alloy. The result shows that an improvement in the mechanical properties of the processed zone is accomplished due to grain and second phase particles refinement. The hardness of the multi-pass FSP (M-FSP) sample is about HV 40 higher than that of the base metal. And the tensile strength of the M-FSP specimens is also significantly increased to about 1.4 times that of the base metal. Besides, the weak region of the processed zone is mainly dependent on the moving distance, where it is the previous pass stir zone in the traditional way and the transitional zone in the novel way. Increasing the rotational speed narrows the weak region in the novel way, while it does not in the traditional way.
Talk to us
Join us for a 30 min session where you can share your feedback and ask us any queries you have
More From: Transactions of Nonferrous Metals Society of China
Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.