AbstractTwo series of copolymers were synthesized by emulsion polymerization: poly(styrene‐co‐acrylonitrile) P(S:AN) and P(S:AN‐acrylic acid) P(S:AN‐AA). The monomeric concentrations in both series were: 0:100, 20:80, 40:60, 50:50 (wt%:wt%), and 1 wt% of AA. The copolymers were dissolved in N,N‐dimethylformamide (4–10 wt%) and were electrospun. Polymeric yarns were collected using a blade collector. The synthesized and fabricated materials were characterized by known techniques. Mechanical and electrical properties of polymeric yarns indicated a dependence of monomeric concentration. Elastic modulus increases as acrylonitrile concentration increases (up to 30 MPa). Yarns were submitted to degradation process into saline solution, where the acrylic acid content kept a constant elastic modulus at long times. The electrical current into yarns was higher when the concentration is 50:50 wt%:wt% (1.2 mA). The cytotoxicity results showed a cell viability close to 100% for yarns without AA.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.