Abstract
WC-MgO whisker composite (abbreviated as WC-MgOw composites) has been sintered by hot pressing. The purpose of present study is to investigate the influence of various content of MgO whisker addition on mechanical performance of WC-MgOw composites. Vickers hardness and fracture toughness of WC-MgOw composites first increase and then decrease with the addition of MgO whisker. The optimal values of Vickers hardness and fracture toughness are achieved, respectively 20.92 GPa and 9.85 MPa m1/2, when the MgO whiskers content reaches 1 wt%. The fracture toughness of WC-MgOw composite is about higher 10.2% than the sample's without MgO whiskers. However, the relative density of the WC-MgOw composites decreases continuously with the addition of MgO whiskers. When the content of MgO whisker is relatively high, the fracture mode is changed and large pores appear. Thus, the mechanical properties of WC-MgOw composite is decreased. The main toughening mechanisms can attribute to crack deflection, crack bridging and whisker pull-out. The mixture of intergranular and transgranular fracture mode also increase the fracture toughness.
Talk to us
Join us for a 30 min session where you can share your feedback and ask us any queries you have
Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.