Abstract

Chromium cast irons (CCI) comprise versatile materials that encompass a range of compositions and microstructures often chosen to promote good wear resistance. There are, however, issues that arise when the cast iron is required to operate in conditions where corrosion, as well as, wear is a factor. This scenario usually results in adapting the composition of the CCI in order to achieve higher chromium content in the metallic matrix and, thereby, to attain the corrosion resistance exhibited by high-Cr stainless steels. This paper comprises a comparison of the corrosive wear behaviour of an austenitic-based hypoeutectic cast iron and a martensitic-based, near-eutectic cast iron with the associated stainless steels, in a saline water under solid-liquid submerged jet conditions. A comprehensive experimental methodology has been adopted including evaluation of the behaviour of the materials in free erosion-corrosion conditions and with the application of cathodic protection. This approach has extended the understanding of the fundamental deterioration mechanisms in different hydrodynamic conditions and has highlighted the complexities of the mechanical/electrochemical interactions occurring during erosion-corrosion. An important feature is the influence of micro-galvanic interactions at phase boundaries. The impact of the findings has been discussed in terms of CCI alloy selection and corrosion control strategies.

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.