Abstract
The current research focuses on the microstructural analysis, damping, and magnetostrictive behavior of the Fe-12Al and Fe-21Al alloys doped with Tb after various mechanical and heat treatments. The thermomechanical treatment provides enhanced magnetostriction in both Fe-12Al and Fe-21Al with Tb addition. The maximal magnetostriction was observed in the alloys after hot rolling and subsequent 30 min annealing at 900 °C followed by air cooling. Tb increases the low temperature IF background and magnetostriction of Fe-21Al-Tb alloy.
Published Version
Talk to us
Join us for a 30 min session where you can share your feedback and ask us any queries you have
Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.