The results of measurements and experiments on two power plant units are presented. The treated coal is lignite with lower heating values ranging between 9 and 10 MJ/kg and with contents of ash about 20% and moisture about 38%. The influences of significant lignite composition components on heating value, boiler losses, boiler specific production of steam, own consumption of electric power, power consumption for coal grinding and flue gas desulphurisation etc. are discussed. The results of analyses and measurements are graphically presented.

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.