The pitting corrosion of SUSU304 steel can be suppressed by the application of a 19.5 kHz ultrasound (US) in 3.5% NaCl aqueous solution. At a constant vibrator-to-specimen distance of d = 76 mm equal to the wavelength, the suppression effect increased with the input power to vibrator and the largest effect was obtained at the power of I = 8. At constant input powers of I = 2 or 8, the suppression effect decreased with the increase in the vibrator-to-specimen distance, but the largest effect was obtained at d = 68 mm in each case of I = 2 and 8.
Talk to us
Join us for a 30 min session where you can share your feedback and ask us any queries you have
Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.