Abstract

Abstract The objective of this paper was to process a polyamide 6.6 composite reinforced with long glass fibers (50 wt.%) using a design of experiments to determine the processing conditions that simultaneously maximize the flexural strength and the surface quality of the molded composite. The analyzed factors were the barrel temperature profile, the injection speed and the screw speed. To maximize the flexural strength response variable and the surface quality, all studied parameters should be maintained at the higher levels. The analysis of microstructure of composites molded demonstrates that this combination of parameters promotes a greater orientation of the fibers in the outer layers, as well as prevents the migration of glass fiber to surface of the composite. This kind of microstructure is favorable to a better surface quality, and a greater flexural strength.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.