Abstract

In this paper the microstructure evolution of an iron-silicon alloy with 3.2 wt.% silicon throughout the manufacturing stages hot rolling, cold rolling and annealing is presented. Starting with a 35 mm thick feedstock, which was hot rolled to 1 mm, with different cooling conditions, the material was cold rolled to a final thickness of 0.3 mm and final annealed under same conditions to show the influence of the hot rolling on the texture and microstructure of the final annealed material.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.