Abstract
The application of hot isostatic pressing (HIP) on the fine grain MAR-M247 superalloys was investigated for obtaining superior mechanical behaviors. The as-cast samples with grain sizes ranging from 70 to 90 μm were prepared using the fine grain process by varying overheating casting temperatures. Part of test bars was preceded with HIP for comparison. The tensile tests were carried out at elevated temperatures and the fracture morphologies were observed using scanning electron microscopy. The experimental results show that the tensile strengths and elongations of the as-cast fine grain MAR-M247 superalloys are deteriorated due to the presence of microporosity resulting from the liquid metal solidification and contraction. The microporosity can be eliminated by HIP and the tensile strengths and elongations are significantly improved. Nevertheless, the yield strengths of the fine grain MAR-M247 superalloys after HIP decreases because of the formation of coarsened γ′ phase at high temperature and high pressure during HIP. On the other hand, the mechanical behaviors at elevated temperatures are degraded due to the growth of γ′ precipitates around 760 °C.
Talk to us
Join us for a 30 min session where you can share your feedback and ask us any queries you have
Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.