Abstract
AbstractRecent investigations paved the way for hot dip galvanizing in the field of bridge constructions [1]. Due to technical limitations of hot dip galvanizing, steel girders longer than 16 meters have to be divided and connected afterwards. The Chair of Metal Structures works in cooperation with the Chair of Concrete Structures of the Technical University of Munich (TUM) and the Bundesanstalt für Materialforschung und ‐prüfung (BAM), to develop a grouted joint connection, which is suitable for hot dip galvanizing. In contrast to welding the segments on site or using prestressed bolt connections, the hot dip galvanization of the grouted joint remains undamaged for the whole service life time of the structure. As part of this research, the main component of the grouted joint ‐ a hot dip galvanized T‐stud ‐ is investigated regarding its fatigue behaviour. The present paper outlines the idea and the structure of the grouted joint and classifies the hot dip galvanized T‐stud according to a fatigue class given in EN 1993‐1‐9 [2]. Furthermore, the fatigue assessment for the grouted joint and an optimization of the geometry of the T‐Studs is carried out using finite element analysis.
Talk to us
Join us for a 30 min session where you can share your feedback and ask us any queries you have
Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.