In the TC4 titanium alloy subject to high pulsed magnetic field, the phase transformation from α to β occurs. When the magnetic induced intensity increased from 2T, 3T to 4T with constant 30 pulses, the percent of α phase adds up gradually. When the magnetic induced intensity is 4T the volume fraction of α phase amounts up to 59%. It is ascertained that magnetic field has taken a positive influence on the phase transformation because of the variation of inner energy induced by magnetic field.