The paper presents results of the electrochemical corrosion resistance tests of the fine-crystalline strips made of the Ni 3 Al intermetallic phase base alloys with the chemical composition in % at.: Ni – 22.13Al – 0.26Zr – 0.1B. Subject of the analysis was a material in the state of strain hardening to 50% deformation, as well as after one-hour annealing in the 600, 700, 800 and 1100 °C temperatures. An influence of the heat treatment temperature at the obtained electrochemical parameter values and correlation of the changes with recovery and recrystallisation processes observed in the material have been found.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.