Abstract

In this paper the tensile and fatigue life tests of carbon fiber-reinforced epoxy prepreg (CFRP) were conducted in order to investigate the influence of volume ratio and fiber orientation. CFRP/Al7075 laminate hybrid composite (CARALL) consists of alternating Al7075-T6 sheets and carbon epoxy prepreg (epoxy 121oC #2560). The fiber orientations of CFRP were applied to the extent of 0/90° and ±45°. The CFRP layers are 1ply, 3plies and 5plies in case of 0/90°, and 1ply and 2plies in case of ±45° of carbon fiber direction, respectively. The tensile strength decreased with the volume ratio of CFRP in both the cases of fiber orientation 0/90° and ±45°. The fatigue life is lower in large volume ratio of CFRP than in small volume ratio in both the cases of fiber orientation 0/90° and ±45°.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.