We report a process of fabrication of latex tubes using the dip-coating technique. We investigated centrifuged latex, with different original viscosities, extracted from the Hevea brasiliensis. The influence of the main deposition parameters (dip-coating velocity, mold material, mold diameter and number of coatings) and post-deposition drying process parameters (temperature and time) on the properties of the final samples are investigated and discussed. Additional investigation about the elastic behavior of the tubes is presented for strain values up to rupture. The rupture occurred at 120 mm for tubes 15 mm-long, which represents an elongation of 800%. The tubes presented two distinct elastic mechanisms, with the most elastic one being observed below an elongation of about 500%. During a cycled strain experiment with strain values below the rupture point, a hysteretic-like curve was observed, which was related to the uncurling and recurling of the polymeric chains.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.