AbstractThree types of poly (vinylidene fluoride‐hexafluoropropylene) (PVDF–HFP) copolymer films were prepared by extrusion, stretching as well as simultaneously stretching and static electric field poling (SSSEP), respectively, and measured by the differential scanning calorimetric, wide angle X‐ray diffraction, fourier transformation infrared‐attenuated total reflection, and Dynamic mechanical analysis. The experimental results showed that the films prepared by stretching and SSSEP have higher crystallinity and β phase than by extrusion. SSSEP improved the chain orientation enormously both in crystalline and amorphous regions, resulting in the highest storage modulus. Because of the lower β phase content, the extruded films exhibited the lowest piezoelectric coefficient d33. For the stretched and SSSEP films, although the β phase content was similar, the d33 was distinct because of the different potential energy for the rotation of the dipoles. In addition, the SSSEP films gave the maximum d33 (24 pC/N), higher than the other PVDF–HFP copolymer films that have been reported. © 2007 Wiley Periodicals, Inc. J Appl Polym Sci 104: 858–862, 2007

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.