We investigated the effect of thulium ion concentration on the continuous-wave (CW) power performance of diode single-end-pumped thulium-doped YAlO/sub 3/ (Tm:YAP) lasers. Three samples with 1.5%, 3%, and 4% Tm/sup 3+/ concentration were examined at 18/spl deg/C. Lifetime and fluorescence measurements were further performed to assess the strength of cross relaxation and nonradiative decay. Our results showed that in single-end-pumped configurations, the best CW power performance was obtained with the 1.5% Tm:YAP sample, and laser performance of the samples degraded monotonically with increasing Tm/sup 3+/ concentration. By using 9.5 W of incident pump power at 797 nm, a maximum of 1430 mW of output power was obtained with the 1.5% Tm:YAP sample and 2% output coupler. We discuss how the effects of cross relaxation, reabsorption, nonradiative decay, and internal heating vary with increasing concentration. Spectroscopic measurements and rate-equation analysis suggest that cross relaxation should already be effective in samples with 1.5% Tm/sup 3+/ ion concentration and doping concentrations larger than 4% will lead to degradation in power performance due to higher nonradiative decay rates and larger reabsorption losses.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.