Abstract
The aim of the study was to evaluate the microtensile bond strength of a composite resin to dentin modified with three different pulse durations of the Er:YAG laser based on variable square pulse technology and with one self-etch adhesive. The entire occlusal enamel was removed to obtain flat dentin surface for 48 human molar teeth. The teeth were randomly divided into four experimental groups (n=12 per group), according to the pretreatment of dentin: (1) control group; (2) super short pulse (SSP) (50 μsec); (3) medium short pulse (MSP) (100 μsec); and (4) short pulse (SP) (300 μsec) with Er:YAG laser. The energy of the laser used was 80 mJ with average power of 0.8 W. The microtensile bond strength was tested with a universal testing machine. Two specimens from each experimental group were subjected to scanning electron microscopic (SEM) examination, to observe the irradiated surface. Dentin surface treated with SSP showed significantly lower microtensile bond strength values (24±9.8 MPa) in comparison with the control group and SP group (35.3±12.8 and 32.9±10.7 MPa, respectively), (p<0.05). The MSP and SP groups did not show any statistically significant difference in microtensile bond strength in comparsion with the control group (p>0.05). The use of SP and MSP of the Er:YAG laser with one step self-etch adhesive does not impair or improve the microtensile bond strength in dentin, whereas SSP may not be suitable for dentin surface treatment prior to bonding procedures.
Talk to us
Join us for a 30 min session where you can share your feedback and ask us any queries you have
Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.