Abstract

Wood is a widely used material in the construction sector, both in structural and non-structural applications. Tropical species are appreciated for their high quality and durability in furniture, outdoor and indoor claddings and floors. However, limited information exists about fire reaction of tropical wood. Density is one of the factors that influence the rate of pyrolysis reactions and consequently the charring rate. However, other wood characteristics such as the mineral content also exert an influence on the pyrolysis combustion of wood. Hardwoods present a complex morphological structure and a significant amount of minerals, extracts and exudates. In this work, we study the fire reaction of seven species of tropical hardwood using various fire tests. Results are compared from one test to other one and are discussed in relation with physicochemical properties of wood species. The results show that although there is some correlation between high density and ignition time, parameters such as morphology and mineral content are also relevant.

Full Text
Published version (Free)

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call