The brightness of single-crystal cathodes of LaB6 oriented in the 〈100〉, 〈110〉, and 〈111〉 directions and six other random directions has been measured. The 〈111〉 cathodes produced currents and brightnesses significantly lower than all other orientations. The other orientations studied produced maximum brightnesses in the range 0.7–1.0 MA/cm2 sr, although the 〈100〉 orientation consistently produced currents higher than other orientations and brightnesses as high or higher than most orientations. A change in impurity level from 1540 ppm to less than 1 ppm had no statistical effect on brightness for crystals of the same orientation.

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.