Abstract

The influence of different cooling rates on deep levels in 4H-SiC after high temperature annealing has been investigated. The samples were heated from room temperature to 2300°C, followed by a 20 minutes anneal at this temperature. Different subsequent cooling sequences down to 1100°C were used. The samples have been investigated using photoluminescence (PL) and IV characteristics. The PL intensities of the silicon vacancy (VSi) and UD-2, were found to increase with a faster cooling rate.