In this work, we investigated magnetic properties and magnetocaloric effect in Fe90-xCoxZr7Cu1B₂ (x = 0, 1, 2, 3 and 4) melt-spun ribbons. The ribbons were prepared by using a melt-spinning method with a tangential velocity of a copper wheel of 40 m·s-1. The obtained ribbons are almost amorphous. The alloys exhibit typical soft magnetic behavior with low coercivity at room temperature. A minor replacement of Fe by Co gives an increment in Curie temperature (TC) of the alloys to higher temperatures. The TC of the alloys increases from 242 to 342 K with an increase of x from 0 to 4. Maximum magnetic entropy change, ΔSm max, of the alloys, was found to be larger than 0.7 J·kg-1·K-1 in a magnetic field change ΔH of 12 kOe for all the concentrations of Co. High refrigerant capacitys (RC >100 J ·kg-1 with ΔH = 12 kOe) at room temperature region have been obtained for the alloys. The large magnetocaloric effect near room temperature suggests that the alloys can be considered as magnetic refrigerants in the range of 250-350 K.

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.