1. In Fe-Cr-5% Al alloys the recrystallization temperature increases with an increase in chromium content in the ferrite. 2. The temperature range of heat treatment corresponding to the maximum plasticity of the alloys narrows from 400 to 100°C with an increase in the chromium content in the solid solution from 15 to 45%. 3. The range of allowable grain sizes providing high plasticity of the alloys narrows from 20–80 to 20–50 μm with an increase in chromium content in the solid solution from 15 to 45%.

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.