Abstract
In this study, forty-eight different chenille yarns are produced on a chenille machine using a range of material types, twists, and gauges. In the first group, 4 Nm count chenille yarns are produced with six different pile materials, two different twists, and two different gauges. In the second group, 6 Nm count chenille yarns are produced with the same machine and material parameters. In order to measure the performance of chenille yarns, their abrasion resistance is measured with a chenille yarn abrasion device, and the abrasion resistance of upholstery fabrics made from these yarns used as filling is measured with a Martindale wear and abrasion tester. The results of pile loss are evaluated according to material type, twist, and pile length of the chenille yams. Clearly, there is an improvement in abrasion resistance with increasing twist, gauge (pile length), and the use of natural fibers as pile materials, which may be due to increasing frictional behavior between the pile and lock yarns.
Talk to us
Join us for a 30 min session where you can share your feedback and ask us any queries you have
Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.