Abstract

AbstractWet powder pouring (WPP) was developed as an alternative near net shape process to metal injection moulding (MIM). The amount of binder, which is necessary to obtain a sufficient green strength, is relatively low (2–5 vol.-%) compared to the amount used in the MIM process (about 30 vol.-%). This is advantageous with respect to short debinding times and low residual carbon and oxygen contaminations. A further reduction of the binder content or the application of the WPP process to new materials would be promoted by an understanding of the dependence of green strength on particle characteristics and binder content. In the present investigation the green strengths of stainless steel WPP parts were determined for different particle size distributions and different binder contents (2–8 vol.-%). The green strength was in the range 3 to 7 MN m−2 and the fracture mode was always brittle. A simple fracture mechanical model was developed, which was able to explain the observed relations between binder conte...

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.