Transition metal (TM) dissolution from oxide cathode materials is a major challenge limiting the performance of modern Li-ion batteries. Coating the cathode materials with thin protective layers has proved to be a successful strategy to prolong their lifetime. Yet, there is a lack of fundamental understanding of the working mechanisms of the coating. Herein, the effect of the most commonly employed coating material, Al2O3, on suppressing hydrofluoric acid(HF)-induced TM dissolution from two state-of-the-art cathode materials, LiMn2O4 and LiNi0.8Mn0.1Co0.1O2, is investigated. Karl Fischer titration, fluoride selective probe and inductively coupled plasma optical emission spectrometry are coupled to determine the evolution of H2O, HF and TM concentrations, respectively, when the active materials come in contact with the aged electrolyte. The coating reduces the extent of TM dissolution, in part due to the ability of Al2O3 to scavenge HF and reduce the acidity of the electrolyte. Delithiation of the cathode materials, however, increases the extent of TM dissolution, likely because of the higher vulnerability of surface TMs in +IV oxidation state towards HF attack. In conclusion, the current study evidences the important role of acid-base reactions in governing TM dissolution in Li-ion batteries and shows that coatings enhance the chemical integrity of the cathode towards an acidic electrolyte.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.