The mechanical properties of a 08GBYu sheet steel ((wt %) 0.08 C, 1.0 Mn, 0.04 Nb, 0.04 Al) with a zinc coating and after its electrolytic removal are studied. The mechanical properties of the galvanized steel are shown to change insignificantly in the strain rate range from 8.3 × 10–5 to 25 × 10–3 s–1. The fatigue limit under repeated tension is 400 MPa. The strength properties and the fatigue limit of the steel base increase by 11–13% after electrolytic removal of the coating. The load on an indenter is determined to analyze the hardness of both the coating and the steel with the coating.

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.