Induced ac losses and magnetization curves measured at 4·2 K, are reported for a reversible supersaturated solid solution of Pb-11% Sn, and for the same material after the precipitation of pinning centres. The results show lower hysteretic losses in the precipitated material for peak applied fields up to Hfp, as defined by slow-swept magnetization measurements, but more significantly the losses up to this field are lower than in pure lead.
Talk to us
Join us for a 30 min session where you can share your feedback and ask us any queries you have
Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.