Films of indium selenide was deposited onto glass and indium tin oxide coated glass substrates in acidic medium using chemical bath deposition at room temperature. Indium sulphate and sodium selenosulphate were used as precursors of In3+ and Se2−, respectively. The structural, surface morphological and optical properties of the deposited films were studied. Diffractograms in structural study revealed the deposited material is In2Se3 films. Controlled bath conditions resulted in the evolution of the In2Se3 microrod-like morphology. The optical band gap of the film was found to be 1.7 eV.